This is the current revision of this page, as edited by Citation bot (talk | contribs) at 16:36, 27 April 2024 (Altered date. | Use this bot. Report bugs. | Suggested by Whoop whoop pull up | Category:Aluminium–magnesium–silicon alloys‎ | #UCB_Category 4/15). The present address (URL) is a permanent link to this version.

(diff) ← Previous revision | Latest revision (diff) | Newer revision → (diff)

6009 Aluminium alloy has minor elements as silicon, iron, magnesium, zinc, manganese, copper, chromium, and titanium.[1]

Chemical Composition

[edit]
Element [1] Weight Percentage (%)
Aluminum 95.7 - 98.7
Silicon 0.60 - 1
Iron ≤ 0.50
Magnesium 0.40 - 0.80
Zinc ≤ 0.25
Manganese 0.20 - 0.80
Copper 0.15 - 0.60
Chromium ≤ 0.10
Titanium ≤ 0.10
Remainder (each) ≤ 0.050
Remainder (total) ≤ 0.15

Mechanical Properties

[edit]
Properties [1] Metric
Tensile strength 230 MPa
Yield strength 125 MPa
Elongation at break 25%
Elastic modulus 69 GPa
Shear modulus 26 GPa
Poisson's ratio 0.33

Thermal properties

[edit]
Thermal Properties Metric
CTE, linear 21.6 μm/m-°C at Temperature -50.0 - 20.0 °C
Specific Heat Capacity 0.890 J/g-°C
Thermal Conductivity 172 W/m-K
Melting Point 588 - 650 °C
Solidus 588 °C
Liquidus 650 °C